Call us: 08045478608
Specification
Composition | Epoxy resin steel-filled |
Specific Properties | viscous |
Colour after curing | dark-grey |
Density of the mixture (200g preparation) | 2.75 g/cm3 |
Consumption at a coating thickness of 1,0 mm | 2,75 kg/m2 |
Maximium layer thickness for each working step | 10 mm |
Pot life at +20 deg C (+68deg F) 200g preparation | 60 min. |
Curing time mechanical loads | 16 h |
Final hardness after | 24 h |
Pressure | 110 Mpa |
Pull | 21 Mpa |
Bending | 52 Mpa |
Shore D (ATSM D 1706) | 90 |
Shrinkage | 0.03 % |