Call us: 08045478608
Specification
Composition | Epoxy resin and plastic-filled |
Composition | Pasty |
Colour after curing | grey-green |
Density of the mixture | 1,9 g/cm3 |
Gap bridging max. | 15 mm |
Processing temperature | +10 to +40 deg C |
Curing temperature | +8 to +65 deg C |
Polt life for 25gr preparation and +20 degC (+68 degF) | 30 min. |
Handling strength (35%) after | 60 min. |
Mechanical loads (50% strength) after | 240 min. |
Final strength (100%) after | 48 h |
Pressure (DIN 53281-83) | 80 N/mm2 |
Medium shear strength after 7 days at +20 deg C (+65 deg F) DIN 532832 at | Steel sandblasted: 7,5 N/mm2 |
Shore hardness D | 80 |
Thermal conductivity (ASTM D 257) | 0,5 W/m.K |
Linear shrinkage | <1 % |
Temperature resistance | -50 to +280 briefly +150 deg C |
ISSA-Code | 75.530.06/07 |
IMPA-Code | 81 29 77/78 |