Specification
Basis | Epoxy resin mineral-filled |
Texture | Pasty |
Colour after curing | White |
Mixing ratio by weight (resin/hardener) | 1:1 |
Density of the mixture | 1.9 g/cm3 |
Gap bridging up to max. | 15 mm |
Processing temperature | +10 bis +40 deg C |
Curing temperature | +6 bis +40 deg C |
Pot life for 25g preparation and +20 deg C (+68 deg F) | 4 min. |
Handling strength (35% strength) after | 15 min. |
Capable of bearing mechanical loads (50% strength) after | 60 min. |
Final strength (100% strength) after | 24 h |
Pressure | 40 N/mm2 |
Medium tensile shear strength after 7 days at +20 deg C (+68 deg F) acc. to DIN 532832 on | steel, sandblasted: 6.5N/mm2 |
Shore hardness D | 70 |
Thermal conductivity (ASTM D 257) | 0.40 W/m.K |
Dielectric strength (ASTM D 149) | 3.0 kV/mm |
Temperature resistance -25 to +120, short-term up to | +150 deg C |
Shrinkage | 0.02 % |